Mitsuru Ueda, Hideharu Mori, et al.
Journal of Polymer Science Part A: Polymer Chemistry
Ta thin films were grown by plasma-enhanced atomic layer deposition (PE-ALD) on Si and SiO2 substrates. The deposition processes and film properties were investigated as a function of various key growth kinetic parameters, including TaCl5 exposure time, atomic hydrogen exposure time, hydrogen flow, and growth temperatures. The growth rate increases with increasing TaCl5 exposure time to saturate at approximately 0.08 Å/cycle. Cl content and resistivity, which are closely related each other, are strong function of H exposure time and growth temperature. Low resistivity and low Cl content films were obtained at a low substrate temperature of 150 °C. Transmission electron microscopy and X-ray diffraction show that the grown films are amorphous. H and Cl contents decrease with increasing annealing temperature and intermixing of Ta and Si substrates was observed only at high annealing temperature of 900 °C. The growth mechanisms and thermal stability of PE-ALD Ta thin films are discussed based upon these results. © 2003 Elsevier Science B.V. All rights reserved.
Mitsuru Ueda, Hideharu Mori, et al.
Journal of Polymer Science Part A: Polymer Chemistry
Shaoning Yao, Wei-Tsu Tseng, et al.
ADMETA 2011
Oliver Schilter, Alain Vaucher, et al.
Digital Discovery
P.C. Pattnaik, D.M. Newns
Physical Review B